TECHNICAL INFORMATION
Catalyst for resin finishing
GENERAL PROPERTIES
- A universal catalyst for curing thermosetting resins in textile finishing
- Can be combined with most softeners, additives and finishing auxiliaries
- Shows minimum yellowing on white fabrics
- Shows minimum colour alteration on dyed or printed material
PHYSICAL PROPERTIES
| Appearance |
Clear, colourless liquid |
| Chemical Constitution |
Organic salt solution |
| pH |
5.5 - 6.5 |
| Density (20°C) |
1.2 - 1.3 g/cm3 |
| Solubility |
Soluble in cold water in all proportions |
| Storage |
Can be stored for at least 12 months in closed containers at ambient temperatures |
PROCESSING
The finishing bath is prepared to almost full volume with the resin and other auxiliaries. The Biocat M
is then prediluted separately in cold water and added lastly to the bath set at pH 5 before finally making to volume.
APPLICATION
The required amount of Biocat M used in he finishing bath, depends primarily on the concentration of the resin as sold.
Recommendations:
Biocat M 30 to 50% of the resin dosage.
Refer to the individual resin technical information data for finishing recipes.
PACKAGING
220 Kg Plastic Drum
Note:
The information is not to be taken as a warranty or representation for which we assume legal responsibility nor as permission or recommendation to practice any patented invention without a license. It is offered solely for your consideration, investigation and verification. |
|